Shrinkage, sink marks, and weld lines are different but often interrelated phenomena in injection-molded plastic parts. Shrinkage describes the reduction in volume or dimensions as the polymer cools and solidifies. A sink mark is a local surface depression that often develops above thicker material sections. A weld line forms where separated melt fronts meet again inside the mold.
This distinction matters in Product Design because the causes and countermeasures are not identical. A visible surface defect therefore cannot be explained meaningfully by the machine or material alone. Part geometry, wall thickness, gate position, mold temperature control, packing pressure, and material behavior act together as a system.
Thermoplastics have a higher specific volume in the hot, plasticized state than after cooling. The material therefore contracts as it solidifies. The magnitude of this dimensional change depends, among other factors, on polymer structure, fillers, flow orientation, wall thickness, mold temperature, and process settings.
Shrinkage is therefore not a single universal correction factor that can simply be added to every CAD dimension independently of part and process. For precise interfaces, the actual combination of material, tool concept, flow direction, and tolerance target must be considered. Uneven shrinkage can also cause warpage.
Sink marks typically occur where local material volume is greater and the inner section cools more slowly than the outer skin. If the core continues to shrink after the surface has already solidified, the surface can be pulled inward. Common causes include thick wall sections, overly thick rib or screw-boss connections, and abrupt wall-thickness transitions.
From a design perspective, a consistent wall thickness is therefore more important than simply adding material. Thick sections can be cored out, functions can be supported by slender ribs, and transitions can be designed gradually. Packing pressure and process parameters can influence sink marks, but they cannot compensate for geometry that is unsuitable for molding.
A weld line forms when the melt flow splits, for example around an opening or core or between multiple gates, and the flow fronts later meet again. At this contact zone, two surfaces that have already cooled to some extent must bond. Depending on material, temperature, pressure, and orientation, the line may remain visually visible and may have locally reduced strength.
This is particularly relevant at highly loaded snap hooks, thin webs, sealing zones, or visible high-gloss surfaces. Gate position and flow path should therefore be planned so that critical weld lines are either avoided or shifted into less sensitive areas.
Uniform nominal wall thicknesses, smooth transitions, cored-out thick sections, appropriately dimensioned ribs and bosses, and an early definition of gate position reduce many typical problems. For complex parts, Moldflow or filling simulation can help estimate flow fronts, pressure loss, weld lines, shrinkage, and warpage before tooling begins.
Validation on the real tool remains essential. Material data, machine settings, mold temperature control, and actual surfaces influence the result. The Protolabs Injection Molding Guide likewise describes sink marks, warpage, and weld lines as outcomes of the interaction between geometry and process. Source: Protolabs, Injection Molding Guide – https://www.protolabs.com/resources/guides-and-trend-reports/injection-molding-guide-process-design-tips-materials/
No. Both phenomena can result from unfavorable product geometry even when the tool and machine are fundamentally operating correctly. Conversely, well-designed geometry can still be visibly affected by unsuitable process parameters or mold temperature control.
For a reliable root-cause analysis, design, material, tool, and process should therefore not be assessed in isolation. For visible or safety-relevant areas, documented sample approval with clear acceptance limits is more meaningful than a blanket requirement for a “defect-free” surface.